Polymer Property : Tear Strength = 43.3 kN/m
Polymer Property :
Tear Strength =
43.3 kN/m
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tear Strength
43.3
kN/m
247
pli
Die B,post cured- 2 hours at 177°C; ASTM D624
Multibase C6-350 LH Parts A and B Dow-Corning Class VI Elastomer
Information provided by Multibase