Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 4.52 kN/m | 25.8 pli | |
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application.. |