Polymer Property : Tear Strength = 38.9 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 38.9 kN/m
222 pli
as molded; Die B
Multibase SILASTIC® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 38.9 kN/m
222 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Polyfil HG90 Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 38.9 kN/m
222 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Polyfil HG90 Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..