Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 37.0 kN/m | 211 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Die B |
Momentive Performance Materials Addisilâ„¢ 1060 E Industrial Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Die B |
Momentive Performance Materials Addisilâ„¢ 2060 E Industrial Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Die B |
Momentive Performance Materials Addisilâ„¢ 462 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LIM 8040 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Die B |
Momentive Performance Materials Addisilâ„¢ 460 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 37.0 kN/m @Thickness 1.60 mm |
211 pli @Thickness 0.0630 in |
ISO 34 (Method A) |
SABIC Innovative Plastics ULTEM STM1700 PEI Copolymer Siltem STM1700 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxici.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-70A/B Elastomer KEG2000-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum.. |
|||
Tear Strength | 37.0 kN/m @Thickness 1.60 mm |
211 pli @Thickness 0.0630 in |
ISO 34 (Method A) |
SABIC Innovative Plastics ULTEM STM1700 PEI Copolymer (Europe-Africa-Middle East) Siltem STM1700 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxici.. |
|||
Tear Strength | >= 37.0 kN/m | >= 211 pli | |
Trelleborg Offshore Vikotherm™ 73780 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Formulation Example |
TSE Industries Millathane® 66 Millable Polyurethane Rubber Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical .. |
|||
Tear Strength | 37.0 kN/m | 211 pli | T.D., Split Tear @ 254 mm/min; ASTM D1938 |
Eastman Embrace LV Copolyester for Extruded/Cast Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | ASTM D624 |
ELASTO UK Dryflex® 500750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | ASTM D624 |
ELASTO UK Dryflex® 502750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | ISO 34-B |
AlphaGary Evoprene™ Super G 934 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Formulation Example |
TSE Industries Millathane® 66 Millable Polyurethane Rubber Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical .. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 37.0 kN/m | 211 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 37.0 - 147 kN/m | 211 - 839 pli | Average value: 73.7 kN/m Grade Count:3 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |