Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 36.8 kN/m | 210 pli | Die B, no post cure- press cured for 5 minutes; ASTM D624 |
Multibase SILASTIC® 7-6840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die B, no post cure- press cured for 5 minutes; ASTM D624 |
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 36.8 kN/m | 210 pli | ASTM D624 |
PolyOne Dynaflex™ G7430-9001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B65B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die 'C'; ASTM D624 |
DSM Biomedical PurSil® AL 20 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | ASTM D624 |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tear Strength | 36.8 kN/m | 210 pli | ASTM D624 |
Multibase Multi-Flex® TEA 1004 TPO Thermoplastic Polyolefin Elastomer Features: Adhesion, GoodPaintableWeather Resistance, Good Forms:PelletsUses: Automotive ApplicationsSealsToothbrush HandlesInformation provided by Multibase |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die B,molded-without post cure; ASTM D624 |
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die B,molded-without post cure; ASTM D624 |
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die B,post cured- 2 hours at 177°C; ASTM D624 |
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 36.8 kN/m | 210 pli | ASTM D624 |
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die B |
Shin-Etsu Silicones SV-56000U High Strength Silicone Elastomer SV56000U is one of a series of silicone bases designed for applications requiring high strength. Product Features: Excellent mechanical properties.Typical Applications: Molding and Extrusion applica.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 75-LR-1 TPE Product Description: StarTUFF TF 75-LR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die C; ASTM D624 |
Teknor Apex APEX® 3070-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® TCKGN Heavyweight Rough Surface Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | |
Dow Corning SILASTIC® 7-6840 BIOMEDICAL GRADE LSR, KIT Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning |
|||
Tear Strength | 36.8 kN/m | 210 pli | |
Dow Corning SILASTIC® LC-70-2004 PART A&B KIT 70 Durometer, 2 parts, 1 to 1 mix, translucent, FDA 21 CFR 177.2600 and BfR, XV, molding and injection molding grade Liquid Silicone Rubber. Fast curing speed, long pot life (72 hours), high transpa.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | |
Dow Corning SILASTIC® Q7-4735 BIOMEDICAL GRADE ETR ELASTOMER, KIT Two-part, platinum-catalyzed (1:1 by weight), enhanced tear-resistant silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices.I.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | |
Dow Corning SILASTIC® Q7-4840 BIOMEDICAL GRADE ETR ELASTOMER, KIT Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning |
|||
Tear Strength | 36.8 kN/m | 210 pli | 73°F, Die C, Across Flow; ASTM D624 |
ExxonMobil Santoprene® 121-79W233 Thermoplastic Elastomer A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner .. |
|||
Tear Strength | 36.8 kN/m | 210 pli | ISO 34-1 |
Alliance Polymers Viprene™ G65A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G65A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 36.8 kN/m | 210 pli | ASTM D624 |
Multibase Multi-Flex® A 6502 MR Natural TPE Thermoplastic Elastomer Forms: PelletsInformation provided by Multibase |