Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 33.8 kN/m | 193 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 33.8 kN/m | 193 pli | post cured- 8 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4720 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 33.8 kN/m | 193 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7170-1000 TPE Product Description: StarFlex P 7170-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |