Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 32.8 kN/m | 187 pli | Die B, post cured- 8 hours at 200°C; ASTM D624 |
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 32.8 kN/m | 187 pli | Notched, Die B; ASTM D 624 |
CPT C-Flex® R70-028 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 32.8 kN/m | 187 pli | Die B; Silicone Property; Arlon SQA-TMS-029 |
Arlon T3020-B004 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 1.0 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape.Design/Construction:Side 1: Cured Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Silicone.. |
|||
Tear Strength | 32.8 kN/m | 187 pli | Die B; Silicone Property; Arlon SQA-TMS-029 |
Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 0.5 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number... |