Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 32.1 kN/m | 183 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® C7-4565 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 32.1 kN/m | 183 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tear Strength | 32.1 kN/m | 183 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7070-1000 TPE Product Description: StarMediflex P 7070-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tear Strength | 32.1 kN/m | 183 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Tear Strength | 32.1 kN/m | 183 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |