Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 30.5 kN/m | 174 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8299 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 30.5 kN/m | 174 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 30.5 kN/m | 174 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7380-1000 TPE Product Description: StarFlex P 7380-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tear Strength | 30.5 kN/m | 174 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |