Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 30.4 kN/m | 173 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 30.4 kN/m | 173 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 30.4 kN/m | 174 pli | |
Taiwan PU Corporation CPU-69-A/B Mixing Ratio 100/36 Polyurethane Casting Elastomer Compound of CPU-69-A/B with a mixing ratio of 100/36.Information provided by Taiwan PU Corporation.MatWeb has a separate entry for the unmixed A nd B components. |
|||
Tear Strength | 30.4 kN/m | 173 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 30.4 kN/m | 173 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 30.4 kN/m | 174 pli | kg/cm²; JIS-K-6301 |
Denka LCS Z1060 Thermoplastic Elastomer, Extrusion grade (general) "DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r.. |
|||
Tear Strength | 30.4 kN/m | 173 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured FormulationNordel® IP 5565 |