Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 30.0 kN/m | >= 171 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7150 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 30.0 kN/m | 171 pli | ISO 34-1 |
PolyOne OnFlex™ S KA 60A-3S1769 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tear Strength | >= 30.0 kN/m | >= 171 pli | DIN 53507 |
Karina TR-605-22/23 Crepe PVC Compound PVC compound additivated with nitrile rubber.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 30.0 kN/m | >= 171 pli | DIN 53507 |
Karina TR-605-22/23 Crepe PVC Compound PVC compound additivated with nitrile rubberInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2060 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2671 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2750 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4670 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94305 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | TD; ISO 6383-2 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3386/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-40AB Elastomer KE-2090-40 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die C; ASTM D624 |
Teknor Apex Uniprene® 73A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R439 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R506 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg B739 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R396 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R504 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | ASTM D624 |
ELASTO UK Dryflex® 600600S SEBS Based Material, Filled Qualities, 60A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 30.0 kN/m | 171 pli | ASTM D624 |
ELASTO UK Dryflex® 600650S SEBS Based Material, Filled Qualities, 65A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6 Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | ISO 34-B |
AlphaGary Evoprene™ 007 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | ISO 34-B |
AlphaGary Evoprene™ 3275 Standard SBS Thermoplastic Elastomer Compound |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Silopren™ LSR 4060 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R397 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R847 Natural Rubber Polyisoprene All information provided by Trelleborg |