Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 3.40 kN/m | 19.4 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 9002-SR BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 3.40 kN/m | 19.4 pli | ASTM D624 |
Objet FullCure® 930 Tango Plus Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Tear Strength | 3.40 - 20.0 kN/m | 19.4 - 114 pli | Average value: 6.49 kN/m Grade Count:17 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |
|||
Tear Strength | 3.40 kN/m | 19.4 pli | JIS-K-6252 (Angle)/ASTM D-624 |
Fujipoly Industries Sarcon® GR-HFk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Tear Strength | 3.40 kN/m | 19.4 pli | Die B |
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Tear Strength | 3.40 kN/m | 19.4 pli | Die B |
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |