Polymer Property : Tear Strength = 3.00 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength >= 3.00 kN/m
>= 17.1 pli
Die C; ASTM D624
Rogers Corporation Poron® 4701-60-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Tear Strength 3.00 - 39.4 kN/m
17.1 - 225 pli
Average value: 11.2 kN/m Grade Count:45
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
Tear Strength 3.00 kN/m
17.1 pli
60°C for 1,000 hrs with 90% RH; JIS-K-6252 (Angle)
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over..
Tear Strength 3.00 kN/m
17.1 pli
ISO 8067
Zotefoams ZOTEK® N B50 High Performance Nylon Foam
Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Tear Strength 3.00 kN/m
17.1 pli
Dow Corning 736 HEAT RESISTANT/SEALANT
Red RTV adhesive/sealant for temperatures up to 600F/315CInformation provided by Dow Corning
Tear Strength 3.00 kN/m
17.1 pli
T.D., Split Tear @ 254 mm/min; ASTM D1938
Eastman Embrace LV Copolyester for Shrink Film
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo..
Tear Strength 3.00 kN/m
17.1 pli
ACC MM709 Low Tear Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh..
Tear Strength 3.00 kN/m
17.1 pli
ACC MM810 Low Tear Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh..
Tear Strength 3.00 kN/m
17.1 pli
ACC MM830 Low Tear Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh..