Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 29.1 kN/m | 166 pli | Die C, press cure 11 min./160ºC |
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co.. |
|||
Tear Strength | 29.1 kN/m | 166 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 29.1 kN/m | 166 pli | Die C, press cure 11 min./160ºC |
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co.. |
|||
Tear Strength | 29.1 kN/m | 166 pli | |
Dow Corning SILASTIC® LS 5-8761 FLUOROSILICONE RUBBER BASE 67 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tear Strength | 29.1 kN/m | 166 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 191-85PA Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft .. |
|||
Tear Strength | 29.1 kN/m | 166 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |