Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 27.5 kN/m | 157 pli | Die B, post cured- 4 hours at 200°C; ASTM D624 |
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 27.5 kN/m | 157 pli | ASTM D624 |
Network Polymers Softflex® 5300 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 27.5 kN/m | 157 pli | ASTM D624 |
Network Polymers Softflex® 5500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 27.5 kN/m | 157 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 27.5 kN/m | 157 pli | Die B, no post cure; ASTM D624 |
Multibase C6-530 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 27.5 kN/m | 157 pli | 500 mm/min; ASTM D 624 |
Zylog Neoplast® 173 C Thermoplastic Vulcanizate Neoplast 173 C is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV S.. |
|||
Tear Strength | 27.5 kN/m | 157 pli | 500 mm/min; ASTM D 624 |
Zylog Neoplast® 173 FT EB Thermoplastic Vulcanizate Neoplast 173 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Tear Strength | 27.5 kN/m | 157 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 27.5 kN/m | 157 pli | |
Dow Corning 25150-G SILICONE RUBBER Peroxide cured, general purpose silicone rubber compoundInformation provided by Dow Corning |