Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 239 kN/m | 1360 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Tear Strength | 239 kN/m | 1360 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |