Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Multibase Multi-Flex® RP 6568 C Natural TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Multibase Multi-Flex® A 6221 CUV Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 9100-45 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B |
Shin-Etsu Silicones KE-5530U Low Temperature Silicone Elastomer ShinEtsu KE5530 U is a nominal 30 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D470 |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning HS II BASE & 10:1, COLORED CATALYST High strength silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items and better suited for thin section cure. HS II Base with HS II 10:1 Colored C.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C; ASTM D 624 |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C; ASTM D 624 |
CPT C-Flex® R70-051 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning SILASTIC® LS 4-9060 FLUOROSILICONE RUBBER 60 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning SILASTIC® P-1 RTV SILICONE RUBBER & BLUE CURING AGENT High strength silicone rubber suited for prototyping, production tooling, artistic and renovation applications. Silastic P-1 is recommended for use with polyesters, cement and rigid polyurethanes; a.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning SILASTIC® S-2 RTV SILICONE RUBBER BASE & CURING AGENT High strength, lower durometer silicone rubber suited for many moldmaking applications. Silastic S-2 is recommended for use with plaster, cement and rigid polyurethane and can be used with polyester.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B, Silicone Property; ASTM D624 |
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B, Silicone Property; ASTM D624 |
Arlon 31560R015 0.015" (0.381 mm) Uncured Silicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE Carrier This data represents typical values for the production material. The data should not be us.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 5 Industrial PTFE-Coated Glass Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, gas.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Multibase Multi-Flex® A 6221 CUV A Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Multibase Multi-Flex® A 6221 CUV A VY Dk Pewter TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® ST-6350 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |