Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 22.6 kN/m | 129 pli | post cured- 4 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4780 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | <= 22.6 kN/m | <= 129 pli | Die C; Formulation Example; Press Cure 7'/177ºC |
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot.. |
|||
Tear Strength | 22.6 kN/m | 129 pli | ASTM D412 |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Tear Strength | <= 22.6 kN/m | <= 129 pli | Die C; Formulation Example; Press Cure 7'/177ºC |
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot.. |
|||
Tear Strength | 22.6 kN/m | 129 pli | |
Dow Corning SILASTIC® LC-20-2004 PART A&B KIT 20 Durometer, 2 parts, 1 to 1 mix, translucent, FDA 21 CFR 177.2600 and BfR, XV, molding and injection molding grade Liquid Silicone Rubber. Fast curing speed, long pot life (72 hours), high transpa.. |
|||
Tear Strength | 22.6 kN/m | 129 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-12 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 22.6 kN/m | 129 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |