Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 215 kN/m | 1230 pli | ASTM D624 |
BASF Elastollan® C-60D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue.. |