Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 21.9 kN/m | 125 pli | Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Die B |
Shin-Etsu Silicones KE-5560U Low Temperature Silicone Elastomer ShinEtsu KE5560 U is a nominal 60 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Fill/Transverse direction |
Saint-Gobain Chemlam® RL® RL1000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sint.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Fill/Transverse direction |
Saint-Gobain Chemlam® RL® RL7000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sint.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Initial Tear Strength |
Saint-Gobain CHR® SGC6-06(R) CHEMLAM Copper Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 5 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 5 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | |
Shin-Etsu Silicones KE-1300T Silicone, Mold Making RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tear Strength | 21.9 kN/m | 125 pli | |
Shin-Etsu Silicones KE-1310ST Silicone, Mold Making RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Die B |
Shin-Etsu Silicones KE-5550U Low Temperature Silicone Elastomer ShinEtsu KE5550 U is a nominal 50 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Die B |
Shin-Etsu Silicones KE-5570U Low Temperature Silicone Elastomer ShinEtsu KE5570 U is a nominal 70 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | ASTM D624 |
DuPont Keldax® 6868 Filled Thermoplastic Ethylene Polymer A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Trouser; ASTM D470 |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Die B, Silicone Property; ASTM D624 |
Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT38-004M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeTransparentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Choic.. |
|||
Tear Strength | 21.9 kN/m | 125 pli | ASTM D470 |
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E.. |