Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.6 kN/m | 118 pli | at 25°C |
Daikin DAI-EL G-555 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |
|||
Tear Strength | 20.6 kN/m | 118 pli | at 25°C |
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries. |
|||
Tear Strength | 20.6 kN/m | 118 pli | at 25°C |
Daikin DAI-EL G-551 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |
|||
Tear Strength | 20.6 kN/m | 118 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-11 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 20.6 kN/m | 118 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |