Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.5 kN/m | 117 pli | ASTM D624 |
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Tear Strength | 20.5 kN/m | 117 pli | ASTM D624 |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tear Strength | 20.5 kN/m | 117 pli | JIS K6301-B |
Stellarchem GP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Tear Strength | 20.5 kN/m | 117 pli | at 25°C |
Daikin DAI-EL G-558 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low gasoline permeability and good.. |
|||
Tear Strength | 20.5 kN/m | 117 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ HTE 1106 Styrene Butadiene Block Copolymer (SBC)