Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.0 - 25.0 kN/m | 114 - 143 pli | |
Prodways PLASTCure Flex 100 3D Printing Polymer High workability. Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Suitable for the manufacture of flexible objects for.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene LDPE 2100TN00: Heavy duty film suitable for application in shrink hoods, industrial sacks, heavy duty carrier bags and liners.Information provided by Iran Petrochemical Commercial Co. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FSL 7651 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials HV 3/806 Heat Cured Rubber - High Temperature Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Shin-Etsu Silicones KEG-2000-20A/B Elastomer KEG-2000-20 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg B429 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg Neoprene® C423 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg Neoprene® C627 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg Neoprene® C738 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg Neoprene® C739 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg Neoprene® C856 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg R408 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg R480 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg S765 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg E701 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg S761 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 20.0 kN/m | 114 pli | ASTM D624 |
ELASTO UK Dryflex® 400501S SBS Based Material, 50A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ASTM D624 |
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | at 25°C |
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing .. |
|||
Tear Strength | 20.0 - 30.0 kN/m | 114 - 171 pli | Die B; ASTM 624 |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Tear Strength | 20.0 - 30.0 kN/m | 114 - 171 pli | Die B; ASTM 624 |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5688 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |