Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 2.00 - 113 kN/m | 11.4 - 645 pli | Average value: 24.8 kN/m Grade Count:768 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | 60°C for 1,000 hrs with 90% RH; JIS-K-6252 (Angle) |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | 150°C for 1,000 hrs; JIS-K-6252 (Angle) |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | 70°C for 1,000 hrs; JIS-K-6252 (Angle) |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | JIS-K-6252 (Angle)/ASTM D-624 |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | 70°C for 1,000 hrs; JIS-K-6252 (Angle) |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | JIS-K-6252 (Angle)/ASTM D-624 |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | 60°C for 1,000 hrs with 90% RH; JIS-K-6252 (Angle) |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | JIS-K-6252 (Angle)/ASTM D-624 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | 150°C for 1,000 hrs; JIS-K-6252 (Angle) |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | 150°C for 1,000 hrs; JIS-K-6252 (Angle) |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | 85°C for 1,000 hrs with 85% RH; JIS-K-6252(Angle); ASTM D 624 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | |
ACC MM828 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | |
ACC MM850 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Tear Strength | 2.00 kN/m | 11.4 pli | |
ACC Silcoset 101 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |