Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 188 kN/m | 1070 pli | ISO 34B |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Tear Strength | 188 kN/m | 1070 pli | ASTM D624 |
Huntsman IROGRAN® A 98 E 4735 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |