Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 185 kN/m | 1060 pli | Graves (initial), TD; ASTM D1004 |
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Tear Strength | 185 kN/m | 1060 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR6650 Modified Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |