Polymer Property : Tear Strength = 18.9 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 18.9 kN/m
108 pli
as molded; Die B
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 18.9 kN/m
108 pli
73°C, Die C; ASTM D624
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Tear Strength 18.9 kN/m
108 pli
Die B, Silicone Property; ASTM D624
Arlon R38081R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured SiliconeInterleave 2: Polyethylene This data represents typical values ..
Tear Strength 18.9 kN/m
108 pli
73°F, Die C; ASTM D624
ExxonMobil Santoprene® 191-70PA Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft ..
Tear Strength 18.9 kN/m
108 pli
73°C, Die C; ASTM D624
ExxonMobil Geolast® 701-70 Thermoplastic Elastomer
A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..