Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 16.0 kN/m | 91.0 pli | 73°F; ASTM D624 |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | Die B |
Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | Die B; DCBP Cure |
Shin-Etsu Silicones KE-551U Silicone Rubber KE551U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | Die C; ASTM D624 |
Teknor Apex Uniprene® 55A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
Tear Strength | 16.0 kN/m | 91.4 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | |
ACC MM911 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tear Strength | 16.0 - 37.0 kN/m | 91.3 - 211 pli | ASTM D 624 |
API Megol AM DP2339 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | angle |
Momentive Performance Materials XE23-703U Heat Cured Rubber - Electro Conductive Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R37732W079 0.079" (2.01 mm) Cured Silicone Rubber with Treated FEP Film Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Treated FEP FilmThis data represents typical values for the production material. The data should not be used to w.. |