Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 150 kN/m | 856 pli | ASTM D624 |
GRECO ISOTHANE 1198A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tear Strength | 150 kN/m | 855 pli | Unnicked; ISO 34-1B |
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec.. |
|||
Tear Strength | 150 kN/m | 856 pli | DIN 53515 |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 150 kN/m | 856 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1495RV Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 150 kN/m | 856 pli | DIN 53515 |
Lubrizol ESTANE® 5799 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 150 kN/m | 856 pli | ISO 34 |
Chengdu Polyster CH7563 Thermoplastic Polyether-ester Elastomer (TPEE) Poly-basic block copolymer. Good compatibility with PBT, PET and PA. For blending with PBT, PET and PA to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 150 kN/m | 856 pli | ISO 34 |
Chengdu Polyster H6055 Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Higher melt flow index compared with other grades; good balance of modulus and toughness. Applications requi.. |
|||
Tear Strength | 150 kN/m | 856 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tear Strength | 150 kN/m | 856 pli | notched; ASTM D624 (C) |
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Tear Strength | 150 kN/m | 856 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR5450 Modified Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 150 kN/m | 856 pli | DIN ISO 34-1/Bb |
BASF Elastollan 1154 D KFFC TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tear Strength | 150 kN/m | 856 pli | DIN ISO 34-1/Bb |
BASF Elastollan B 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tear Strength | 150 kN/m | 856 pli | ASTM D624 |
BASF Elastollan® S95A Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tear Strength | 150 kN/m | 856 pli | |
AorTech Biomaterials ECSil™ 60D Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Tear Strength | >= 150 kN/m | >= 856 pli | ISO 34 |
Austin Novel Materials Texalan® 464D Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 150 kN/m | 856 pli | DIN ISO 34-1/Bb |
BASF Elastollan 598 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri.. |
|||
Tear Strength | 150 kN/m | 856 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 150 kN/m | 856 pli | |
AorTech Biomaterials ECSil™ 60D Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |