Polymer Property : Tear Strength = 14.7 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 14.7 kN/m
84.0 pli
ASTM D624
Microcell Composite Company CELLIFF® F-1020ST Polymer Foam
CELLIFF® FOAM is Light & rigid, tenacious & durable. Patterns can be easily molded into the foam surface. We possess the technology to increase surface hardness to meet requirement.Information pr..
Tear Strength 14.7 kN/m
84.0 pli
Notched, Die B; ASTM D 624
CPT C-Flex® R70-116 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..