Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 131 kN/m | 747 pli | |
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta.. |
|||
Tear Strength | 131 kN/m | 750 pli | ASTM D624 |
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens.. |
|||
Tear Strength | 131 kN/m | 750 pli | ASTM D624 |
Huntsman IROGRAN® PS 443-201 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Tear Strength | 131 kN/m | 750 pli | ASTM D624 |
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro.. |
|||
Tear Strength | 131 kN/m | 750 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 183M PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Tear Strength | 131 kN/m | 750 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 183M PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Tear Strength | 131 kN/m | 747 pli | ASTM D624 |
Teknor Apex Monprene® MP-2207B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 131 kN/m | 750 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 1584G PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain SPECIALTY SERIES Belting Products:Dimensional Stability: Width rigidity as well as length stability is maintained by CHEMFAB Specialty Series belting in co.. |