Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 12.0 - 16.0 kN/m | 68.5 - 91.3 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 3G Polytetrafluoroethylene & Graphite Coated Glass Fabric PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon. |
|||
Tear Strength | >= 12.0 kN/m | >= 68.5 pli | DIN 53507 |
Karina 300-40/236 Green PVC Compound For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ Electro 940 Liquid Silicone Rubber - Medium Voltage This LSR elastomer is a medium voltage, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperat.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3696/20 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Tear Strength | 12.0 - 16.0 kN/m | 68.5 - 91.3 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | |
Trelleborg Commercial Neoprene® C798 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | |
Trelleborg R608 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | |
Trelleborg R661 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | Split tear method, TD; ASTM D1938 |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | Split tear method, TD; ASTM D1938 |
Eastman Tritan MP100 Copolyester Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | |
Trelleborg R660 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | |
Trelleborg Z600 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | ISO 34-B |
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |