Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 11.6 - 21.2 kN/m | 66.2 - 121 pli | propogation; ASTM D1922 |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tear Strength | 11.6 - 21.2 kN/m | 66.2 - 121 pli | propogation; ASTM D1922 |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Tear Strength | 11.6 - 21.2 kN/m | 66.2 - 121 pli | propogation; ASTM D1922 |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Tear Strength | 11.6 - 21.2 kN/m | 66.2 - 121 pli | propogation; ASTM D1922 |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tear Strength | 11.6 kN/m | 66.0 pli | Die B; DBPH Cure |
Shin-Etsu Silicones SV-14000U Silicone Rubber SV14000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat.. |
|||
Tear Strength | 11.6 kN/m | 66.0 pli | |
Dow Corning SILASTIC® 37088-V SILICONE RUBBER RED 80 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning |
|||
Tear Strength | 11.6 - 21.2 kN/m | 66.2 - 121 pli | propogation; ASTM D1922 |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |