Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 10.0 kN/m | 57.1 pli | Support Rubber |
Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Insulating Layer |
Fujipoly Industries Zebra® 1002 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Support Rubber |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Insulating Layer |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Support Rubber |
Fujipoly Industries Zebra® 2005 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Support Rubber |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Insulating Layer |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LIM 6010 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2680FC High Productivity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 7070 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Insulating Layer |
Fujipoly Industries Zebra® 2004 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE2004-10A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | |
Trelleborg Hypalon® H630 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | |
Trelleborg Hypalon® H730 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | MD; Trouser @200/mm/min; ISO 6383-1 |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 3005-101 TPE, Modified Injection Molding Grade for Vacuum Cleaner Seals The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3005-101 is specifically designe.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | MD; ASTM D5734 |
3M GM110 Gripping Material 3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM 110 consists of a high-friction surface with a nylon knit backing that provides stretch.. |