Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.93 kN/m | 11.0 pli | Initial Tear Strength; ASTM D624 Die C |
Saint-Gobain Korel® K20 Very Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Tear Strength | 1.93 kN/m | 11.0 pli | |
Dow Corning SILASTIC® LSR 9390-40 PARTS A&B 40 Durometer, 2-part, 1 to 1 mix, off-white, molding grade, Liquid Silicone RubberInformation provided by Dow Corning |