Polymer Property : Tear Strength = 1.21 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 1.21 kN/m
6.90 pli
Split; ASTM D624
Northstar Polymers MPP-A50A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Tear Strength 1.21 - 167 kN/m
6.90 - 950 pli
Average value: 52.9 kN/m Grade Count:26
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Tear Strength <= 1.21 kN/m
<= 6.90 pli
Max.; ASTM D3574
Lendell Nolatex® Latex Free Foam
This foam is used in the cosmetics industry and also possesses insulation qualities.Applications:Cosmetic Wedges and Puffs, Padding, High Insulative Value Applications, Makovers ® Disposable Make..