Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.20 kN/m | 6.85 pli | BS EN ISO 8067 1995 |
Zotefoams Plastazote® LD45FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Tear Strength | 1.20 kN/m | 6.85 pli | Die C; ASTM D624 |
Covestro Bayfill® 380 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Open Pour, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tear Strength | 1.20 kN/m | 6.83 pli | |
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 1.20 kN/m | 6.83 pli | |
3M 12050 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 1.20 kN/m | 6.83 pli | |
3M 12062 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 1.20 kN/m | 6.83 pli | |
3M 12046 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 1.20 kN/m | 6.83 pli | |
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 1.20 kN/m | 6.83 pli | |
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 1.20 kN/m | 6.83 pli | |
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |