Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.01030 GPa @Temperature 1000 °C, Time 10800 sec |
1.494 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories A50 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |