Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0073575 GPa @Temperature 1500 °C, Time 10800 sec |
1.0671 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories A64 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0073575 GPa @Temperature 1000 °C, Time 10800 sec |
1.0671 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories A70 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0073575 GPa @Temperature 110 °C, Time 86400 sec |
1.0671 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories A80 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0073575 GPa @Temperature 110 °C, Time 86400 sec |
1.0671 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories APC-50 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0073575 GPa @Temperature 110 °C, Time 86400 sec |
1.0671 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MMCT-85 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0073575 GPa @Temperature 110 °C, Time 86400 sec |
1.0671 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MMCT-95 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |