Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 0.640 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00441 GPa

@Temperature 1100 °C
0.640 ksi

@Temperature 2010 °F
Sharadaa Ceramics REFCAST A High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Modulus of Rupture 0.00441 GPa

@Temperature 1100 °C
0.640 ksi

@Temperature 2010 °F
Sharadaa Ceramics REFINSUL 4 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..