Modulus of Rupture 0.00165 GPa

@Temperature 104 °C
0.239 ksi

@Temperature 219 °F
Dried; ASTM C268
BNZ Materials Bazelite 2600 LI Insulating Castable
Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov..