Polymer Property : Modulus of Rupture = 0.203 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00140 GPa

@Temperature 1095 °C
0.203 ksi

@Temperature 2003 °F
ASTM C268
BNZ Materials Blazecrete 2500 HS Dense Castable
Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li..
Modulus of Rupture 0.00140 GPa

@Temperature 1095 °C
0.203 ksi

@Temperature 2003 °F
ASTM C268
BNZ Materials Blazecrete 2300 ARG Dense Castable
Blazecrete 2300 ARG is an alumina-silica castable with high strength and abrasion resistance. For service to 2300°F (1260°C). May be gunned or slap-troweled over Blaz 2000G to obtain a high streng..