Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 9.62361e-7 - 0.00981 GPa @Temperature 110 °C, Time 86400 sec |
0.000139581 - 1.42 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HAPT-80S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 9.62361e-7 - 0.006867 GPa @Temperature 1000 °C, Time 10800 sec |
0.000139581 - 0.9960 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SCX-90IP Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |