Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0123 GPa @Temperature 1100 °C |
1.78 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFCAST LC45 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |