Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0070632 GPa @Temperature 110 °C, Time 86400 sec |
1.0244 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories BFSG Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |