Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 13.1 - 108 J | 9.66 - 79.7 ft-lb | Average value: 36.1 J Grade Count:6 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |