Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 10.0 - 10.0 J @Temperature -30.0 - -30.0 °C |
7.38 - 7.38 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 10.0 J Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |