Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 13.0 - 39.0 J @Temperature -40.0 - -40.0 °C |
9.59 - 28.8 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 7.77 J Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |