Polymer Property : Puncture Energy = 81.1 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 110 J
81.1 ft-lb
ISO 6603-2
Lanxess Durethan® BC 30 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, rapid processing, higher notched impact strength than B 30 S / B 31 SK in dry and conditioned state, impact-modified