Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 49.0 J @Temperature -40.0 °C |
36.1 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Puncture Energy | 49.0 J @Temperature -40.0 °C |
36.1 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Puncture Energy | 49.0 - 49.0 J @Temperature -40.0 - -40.0 °C |
36.1 - 36.1 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 49.0 J Grade Count:2 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |